Abstract & Overview

Austenitic stainless steels with excellent corrosion resistance and good weldability have wide applications in industry.These iron-based alloys contain a high level of chromium which form protective oxide film on the surface hence resisting corrosion.The oxide film regenerates when damaged, making the steel 'stainless'.However, carbide precipitation due to a welding process or heat treatment can cause the occurrence of chromium-depleted zones at the boundaries, leading to a phenomenon known as sensitisation, in which the depleted zones become the focus of the intense corrosion.The present work was concerned with the study of the sensitization and desensitisation of 316L steel at the normalizing temperatures of 750-950 0 C and soaking times of 0.5, 1, 2 and 8 hrs.

Cite this record

P. O. Atanda, A. Fatudimu, O.O. Oluwole (2010). Sensitisation Study of Normalized 316L Stainless Steel. Journal of Minerals and Materials Characterization and Engineering, 09(01), 13–23. https://doi.org/10.4236/jmmce.2010.91002

Copy in another style

Atanda, P. O., Fatudimu, A., & Oluwole, O. (2010). Sensitisation Study of Normalized 316L Stainless Steel. Journal of Minerals and Materials Characterization and Engineering, 09(01), 13–23. https://doi.org/10.4236/jmmce.2010.91002
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.