We use a few cookies

Essential cookies keep the library working. With your permission, we'd also like to use analytics to see what's useful and improve the experience. Read our Privacy Policy or Cookie Policy.

Skip to main content
Home/e-Resources/Materials Science/NiAl-30.9Cr-3Mo-0.1Dy合金的微观结构与高温氧化行为
PeriodicalsMaterials Science

NiAl-30.9Cr-3Mo-0.1Dy合金的微观结构与高温氧化行为

Checking your access to this record.

Abstract & Overview

研究了NiAl 30 9Cr 3Mo 0 1Dy合金的微观组织以及在 1300~1500K空气中的恒温氧化行为。实验结果表明,加入微量Dy使合金组织细化,表现为单位体积中共晶团数目增多,Cr(Mo)层片间距减小和Cr(Mo)层片细化。增韧相(Cr(Mo) )与基体相NiAl的互相析出,有利于层状的氧化膜形成,进而提高合金的抗高温氧化性能。合金在 1500K氧化动力学曲线基本上遵循抛物线关系;而氧化温度在 1350~1450K之间,氧化动力学曲线很好地符合立方抛物线关系;当温度为 1300K时,氧化动力学曲线则符合五次方关系。立方抛物线氧化速率常数低于未合金化NiAl的抛物线氧化速率常数,并随着温度降低和氧化时间的延长而逐渐变小,合金的氧化表观激活能为 205kJ/mol。

Cite this record

Author (2005). NiAl-30.9Cr-3Mo-0.1Dy合金的微观结构与高温氧化行为. Hangkong cailiao xuebao, 25(2), 6–11. https://library.shubhaarti.com/content/d06816da-2da5-47e4-9843-2d7d6dc82d4b

Copy in another style

Author. (2005). NiAl-30.9Cr-3Mo-0.1Dy合金的微观结构与高温氧化行为. Hangkong cailiao xuebao, 25(2), 6–11. https://library.shubhaarti.com/content/d06816da-2da5-47e4-9843-2d7d6dc82d4b