Abstract & Overview
Corrosion fatigue specimen with different surfaces (technical surfaces after machining and polished surfaces) of high alloyed martensitic stainless steel X46Cr13 (1.4043) and duplex stainless steel X2CrNiMoN22-3-2 (1.4462) were compared at load amplitudes from 175 MPa to 325 MPa in the geothermal brine of the Northern German Basin at 98 °C. Surface corrosion layers and pits reveal carbonate corrosion products on the surface such as FeCO 3 and FeOOH as the main precipitation phases with no dependence on the original surface roughness. At high stress amplitudes above 275 MPa technical surfaces (P50% at s a 300 MPa=5×10 5 ) resulted in more cycles to failure than polished (P50% at s a 300 MPa=1.5×10 5 ). The greater slope coefficient for technical surfaces k = 19.006 compared to polished surfaces k =8.78 demonstrates earlier failure at given stress amplitude s a .