Abstract & Overview
Can geopolymer concrete serve as a reliable matrix for deep beams reinforced with basalt fiber reinforced polymer (BFRP) bars, and how does the shear span-to-depth ratio influence their load-carrying capacity? This research addressed that question through a controlled experimental programme involving nine deep beam specimens cast with fly-ash-based geopolymer concrete and reinforced longitudinally with BFRP bars of three different reinforcement ratios (0.6%, 0.8%, and 1.2%). The beams measured 1200 mm in overall length, 300 mm in width, and 450 mm in total depth. Three shear span-to-depth ratios (a/d = 0.75, 1.00, and 1.25) were examined, with each ratio tested at all three reinforcement levels. A 12-molar sodium hydroxide activator was blended with sodium silicate solution at a mass ratio of 1:2.5 for the geopolymer binder. Specimens were heat-cured at 65 °C for 24 hours and then left at ambient temperature for 28 days before testing under four-point bending with a 1000 kN universal testing machine. Results showed that ultimate shear capacity ranged from 168.9 kN (a/d = 1.25, ?f = 0.6%) to 371.4 kN (a/d = 0.75, ?f = 1.2%), confirming that lower a/d ratios and higher BFRP reinforcement ratios both contributed to greater shear resistance. Diagonal splitting governed failure at a/d = 0.75, while flexure-shear cracking became more prominent at a/d = 1.25. Raising ?f from 0.6% to 1.2% improved shear capacity by 29.3% at a/d = 0.75 and by 42.8% at a/d = 1.25, pointing to a stronger reinforcement effect when arch action was weaker. The geopolymer matrix displayed crack patterns and stiffness characteristics broadly comparable to those reported for ordinary Portland cement deep beams at similar a/d values, though with marginally wider cracks at peak load.