Abstract & Overview
Through analyzing the number of cross-section cracks of different coating thickness under the same heating process, the same coating thickness under the conditions of different heating temperature, different holding time and different drawing rate, it provides the control direction for decreasing the number of cracks in al-si coating after hot forming process.