The effects of different contents and particle sizes of waste glass powder on alkali–silica reaction (ASR) expansion of cementitious composite bar were investigated in this study. Waste glass powder with particle size less than 300 μm exhibits an excellent mitigation effect on ASR expansion. With larger content and smaller particle size, the mitigation effect of waste glass powder on ASR expansion gradually increases. The mitigation effect of waste glass powder with particle size ranging from 38 to 53 μm and 20% by weight of cement seems relatively better than that of fly ash. When the waste glass powder content reaches 30%, the mitigation effect is still effective and almost the same as that of fly ash. However, the waste glass powder with particle size larger than 300 μm presents negative mitigation effect on ASR expansion when the replacement rate is larger than 30%. On the other hand, the waste glass powder and calcium hydroxide (CH) further react, and produce more calcium–silicate–hydrate gels, which apparently reduce the amount of CH. Moreover, the increasing content of waste glass powder results in a lower pH value in the pore solution of cementitious composite.

Cite this record

Guojun Ke, Wengui Li, Ruyi Li, Yuelin Li, George C. Wang (2018). Mitigation Effect of Waste Glass Powders on Alkali–Silica Reaction (ASR) Expansion in Cementitious Composite. International Journal of Concrete Structures and Materials, 12(1), 67. https://doi.org/10.1186/s40069-018-0299-7

Copy in another style

Ke, G., Li, W., Li, R., Li, Y., & Wang, G. C. (2018). Mitigation Effect of Waste Glass Powders on Alkali–Silica Reaction (ASR) Expansion in Cementitious Composite. International Journal of Concrete Structures and Materials, 12(1), 67. https://doi.org/10.1186/s40069-018-0299-7
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.