Abstract & Overview

KCl was added into rich titanium solution containing Al 3+ to produce KAl(SO 4) 2 as precipitate,Al 3+ in solution was removed.The quantity of KCl and temperature in solution influence deposition ratio of Al 3+ .The results show that precipitation of aluminium cations was more than75% when the mass of KCl was larger than 20% of the solution and temperature was 25℃,75% of Al 3+ was removed.Thus the qualified titanium solution was got .

Cite this record

Ming Wang (2001). Purging Aluminium Cation in Rich Titanium Solution with Potassium Chloride. Multipurpose Utilization of Mineral Resources. https://library.shubhaarti.com/content/d49e70fb-6e8f-4e33-a06f-089c43139899

Copy in another style

Wang, M. (2001). Purging Aluminium Cation in Rich Titanium Solution with Potassium Chloride. Multipurpose Utilization of Mineral Resources. https://library.shubhaarti.com/content/d49e70fb-6e8f-4e33-a06f-089c43139899
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.