We use a few cookies

Essential cookies keep the library working. With your permission, we'd also like to use analytics to see what's useful and improve the experience. Read our Privacy Policy or Cookie Policy.

Skip to main content
Home/e-Resources/Mechanical Engineering/挤压致密超细WC/纳米Al 2 O 3 弥散强化铜基复合材料的组织性能研究
PeriodicalsMechanical Engineering

挤压致密超细WC/纳米Al 2 O 3 弥散强化铜基复合材料的组织性能研究

Checking your access to this record.

Abstract & Overview

以纳米Al2O3颗粒、超细WC粉末、工业纯Cu粉末为原料, 通过热挤压致密获得了超细WC/纳米Al2O3弥散强化铜基(WC-Al2O3/Cu)复合材料, 研究了挤压态WC-Al2O3/Cu复合材料的微观组织及力学性能。结果表明: 成分为5% WC-2% Al2O3/Cu和10% WC-2% Al2O3/Cu (质量分数)的两种原料粉末, 经机械球磨、冷压、真空烧结和热挤压后, 其相对密度均达到了99%以上, 超细WC和纳米Al2O3强化相颗粒呈均匀弥散分布, 具有很好的导电性及力学性能; 其中, 5% WC-2% Al2O3/Cu复合材料的综合性能更佳, 其抗拉强度达到235.06 MPa, 延伸率为15.47%, 导电率可达85.28% IACS, 软化温度不低于900℃。

Cite this record

Author (2019). 挤压致密超细WC/纳米Al 2 O 3 弥散强化铜基复合材料的组织性能研究. 粉末冶金技术, 37(6), 422–427. https://doi.org/10.19591/j.cnki.cn11-1974/tf.2019.06.004

Copy in another style

Author. (2019). 挤压致密超细WC/纳米Al 2 O 3 弥散强化铜基复合材料的组织性能研究. 粉末冶金技术, 37(6), 422–427. https://doi.org/10.19591/j.cnki.cn11-1974/tf.2019.06.004
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.