Abstract & Overview
The introduction of a 15 – 85 wt.% powder of monocalcium phosphate monohydrate Ca(H 2 PO 4 ) 2 · H 2 O into the hydroxyapatite suspension after annealing at 1200°C leads to the formation of resorbable calcium phosphate phases (tricalcium phosphate, calcium pyrophosphate), which makes it possible to control the phase composition of foam ceramics.