We use a few cookies

Essential cookies keep the library working. With your permission, we'd also like to use analytics to see what's useful and improve the experience. Read our Privacy Policy or Cookie Policy.

Skip to main content
Home/e-Resources/Civil & Construction Engineering/Investigation on compressive strength development and drying shrinkage of ambient cured powder-activated geopolymer concretes
PeriodicalsCivil & Construction Engineering

Investigation on compressive strength development and drying shrinkage of ambient cured powder-activated geopolymer concretes

Checking your access to this record.

Abstract & Overview

Geopolymer is an inorganic polymer binding material, generally formed by the reaction between aluminosilicate materials and alkali activator solution. Previous researches on geopolymer concrete around the world suggested that geopolymer concrete possess superior mechanical and durability properties over ordinary Portland cement (OPC) concrete, such as higher indirect tensile strength and resistance to sulphate attack. Generally, fly ash-based geopolymer concrete was cured in elevated temperature for higher early age strength because of their longer setting time in ambient temperature. Published engineering properties of geopolymer concrete cured at ambient temperature are not abundant. In this research, two types of powder-activated geopolymer binders were used as binding material. A detailed study of compressive strength and drying shrinkage of different grades (40, 50, 65 and 80 MPa) of geopolymer and OPC concrete with different workability levels (normal-workable and super-workable) were carried out. All the concrete specimens were cured at standard laboratory temperature. The compressive strength development of geopolymer concrete in early age was relatively lower than OPC concrete; however, the later age strength was significantly higher. The drying shrinkage of geopolymer concrete was similar to OPC concrete of same grade and complied with Australian Standard 1379; however, it was higher than estimated values from Australian Standard 3600. The drying shrinkage results of this study were higher than drying shrinkage of accelerated cured geopolymer concretes in previous investigations. Super workable concrete exhibited higher drying shrinkage than normal workable concrete of same grade.

Cite this record

Kamal Neupane, Paul Kidd, Des Chalmers, Daksh Baweja, Rijun Shrestha (2016). Investigation on compressive strength development and drying shrinkage of ambient cured powder-activated geopolymer concretes. Australian Journal of Civil Engineering, 14(1), 72–83. https://doi.org/10.1080/14488353.2016.1163765

Copy in another style

Neupane, K., Kidd, P., Chalmers, D., Baweja, D., & Shrestha, R. (2016). Investigation on compressive strength development and drying shrinkage of ambient cured powder-activated geopolymer concretes. Australian Journal of Civil Engineering, 14(1), 72–83. https://doi.org/10.1080/14488353.2016.1163765
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.