We use a few cookies

Essential cookies keep the library working. With your permission, we'd also like to use analytics to see what's useful and improve the experience. Read our Privacy Policy or Cookie Policy.

Skip to main content
Home/e-Resources/Biomedical Engineering/Comparative Effect of different Polymerization Techniques on Residual Monomer and Hardness Properties of PMMA-based Denture Resins
PeriodicalsBiomedical Engineering

Comparative Effect of different Polymerization Techniques on Residual Monomer and Hardness Properties of PMMA-based Denture Resins

Checking your access to this record.

Abstract & Overview

PURPOSE: The aim of this study was to compare the residual monomer and microhardness of poly(methyl methacrylate) (PMMA)-based denture resins processed by using autoclave and conventional water bath techniques. METHODS: To determine the amount of residual methyl methacrylate (MMA) monomer, disk-shaped specimens (n=5) were prepared from 3 different acrylic resins (Meliodent, Paladent and Qc-20). Control groups were polymerized in water bath for 30 minutes at 100°C. The study groups were prepared in an autoclave device for 60°C/30 min followed 130°C/10 min and the other group for 60°C/30 min followed by 130°C/20 min. According to standard calibration curves, ultraviolet spectrophotometry at 230 nm was used to determine the residual monomer. For the Vickers hardness measurements, disk-shaped specimens (n=5) were prepared for each test group. Hardness measurements were performed with a Vickers hardness tester under a 4.91-N press load for a 30 seconds, after immersion in distilled water at 37ºC for 48 hours. The data were analyzed by ANOVA and Tukey HSD test (p<0.05). RESULTS: Autoclave polymerization produced a significant decrease in the amount of residual monomers for all resin groups (p<0.05). This procedure also showed a significant increase in hardness for all resin groups (p<0.05). For the 3 resin groups, no significant differences were found between autoclave polymerization for 10 minutes and for 20 minutes (p>0.05). CONCLUSIONS: The autoclave polymerization technique exhibited significantly lower residual monomer content and greater hardness than conventional heat polymerization.

Cite this record

Elif Aydoğan Ayaz, Rukiye Kaplan Durkan, Ayşegül Köroğlu, Bora Bağış (2014). Comparative Effect of different Polymerization Techniques on Residual Monomer and Hardness Properties of PMMA-based Denture Resins. Journal of Applied Biomaterials & Functional Materials, 12(3), 228–233. https://doi.org/10.5301/jabfm.5000199

Copy in another style

Ayaz, E. A., Durkan, R. K., Köroğlu, A., & Bağış, B. (2014). Comparative Effect of different Polymerization Techniques on Residual Monomer and Hardness Properties of PMMA-based Denture Resins. Journal of Applied Biomaterials & Functional Materials, 12(3), 228–233. https://doi.org/10.5301/jabfm.5000199
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.