We use a few cookies

Essential cookies keep the library working. With your permission, we'd also like to use analytics to see what's useful and improve the experience. Read our Privacy Policy or Cookie Policy.

Skip to main content
Home/e-Resources/Materials Science/Effect of in Vitro Enzymatic Degradation on 3D Printed Poly(ε-Caprolactone) Scaffolds: Morphological, Chemical and Mechanical Properties
PeriodicalsMaterials Science

Effect of in Vitro Enzymatic Degradation on 3D Printed Poly(ε-Caprolactone) Scaffolds: Morphological, Chemical and Mechanical Properties

Checking your access to this record.

Abstract & Overview

BACKGROUND: In recent years, the tissue engineering (TE) field has significantly benefited from advanced techniques such as additive manufacturing (AM), for the design of customized 3D scaffolds with the aim of guided tissue repair. Among the wide range of materials available to biomanufacture 3D scaffolds, poly(ε-caprolactone) (PCL) clearly arises as the synthetic polymer with the greatest potential, due to its unique properties - namely, biocompatibility, biodegradability, thermal and chemical stability and processability. This study aimed for the first time to investigate the effect of pore geometry on the in vitro enzymatic chain cleavage mechanism of PCL scaffolds manufactured by the AM extrusion process. METHODS: Methods: Morphological properties of 3D printed PCL scaffolds before and after degradation were evaluated using Scanning Electron Microscopy (SEM) and micro-computed tomography (μ-CT). Differential Scanning Calorimetry (DSC) was employed to determine possible variations in the crystallinity of the scaffolds during the degradation period. The molecular weight was assessed using Size Exclusion Chromatography (SEC) while the mechanical properties were investigated under static compression conditions. RESULTS: Morphological results suggested a uniform reduction of filament diameter, while increasing the scaffolds' porosity. DSC analysis revealed and increment in the crystallinity degree while the molecular weight, evaluated through SEC, remained almost constant during the incubation period (25 days). Mechanical analysis highlighted a decrease in the compressive modulus and maximum stress over time, probably related to the significant weight loss of the scaffolds. CONCLUSIONS: All of these results suggest that PCL scaffolds undergo enzymatic degradation through a surface erosion mechanism, which leads to significant variations in mechanical, physical and chemical properties, but which has little influence on pore geometry.

Cite this record

Joana Cintia Monteiro Ferreira, Antonio Gloria, Stefania Cometa, Jorge F. J. Coelho, Marco A.N. Domingos (2017). Effect of in Vitro Enzymatic Degradation on 3D Printed Poly(ε-Caprolactone) Scaffolds: Morphological, Chemical and Mechanical Properties. Journal of Applied Biomaterials & Functional Materials, 15(3), 185–195. https://doi.org/10.5301/jabfm.5000363

Copy in another style

Ferreira, J. C. M., Gloria, A., Cometa, S., Coelho, J. F. J., & Domingos, M. A. (2017). Effect of in Vitro Enzymatic Degradation on 3D Printed Poly(ε-Caprolactone) Scaffolds: Morphological, Chemical and Mechanical Properties. Journal of Applied Biomaterials & Functional Materials, 15(3), 185–195. https://doi.org/10.5301/jabfm.5000363
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.