Reprocessing of magnesite beneficiation waste to recover mineral value and minimise environmental footprint

Checking your access to this record.

Abstract & Overview

The current paper deals with the re-processing of mineralised mine waste from magnesite processing operations aiming at the recovery of the value. Two cases of mineralised waste were examined. First, waste derived from the removal of “fine” before hand-sorting, with particle size of -40 mm; this waste is usually stockpiled, comprises mostly of relatively coarse particles and is of relatively high-grade in magnesite. The separation methods applied were sorting, sink-float tests and magnetic separation. In general, the results from the application of physical separation methods were satisfactory. Commercial concentrates were obtained from sorting with MgCO3-grade ranging between 94 and 97% MgCO3 and yield about 46%; in case of mixing concentrate with middling, yield rises to 58-64% while grade slightly drops to 91-94%. Equally satisfactory were the results from sink-float separation at sp.gr. 2.88 (grade 95%, yield 45%) but questions arise from the small sp.gr. difference of magnesite and gangues. Finally, the less satisfactory results obtained from magnetic separation (grade around 80-85%, yield 33-65%) may be due to inefficient particles liberation and higher magnetic field is maybe required. Second, mineralised waste consisting of fine particles from size reduction operations were tested. These fines were processed with selective magnetic coating as well as co-agglomeration / magnetic separation techniques. In general, the results of physicochemical processing of fines were very encouraging both on single minerals and their artificial mixtures. In case of magnetic coating, the effect of pH, collector concentration and kerosene dose was studied first on single minerals. Optimum results were obtained for pH=9, dodecylamine solution 4.5x10-5 M and kerosene 2.5 L/t. Tests on artificial mineral mixtures at optimum conditions and magnetic separation at 0.8 A resulted in non-magnetic product with MgCO3-grade higher than 99%. The parameters examined in co-agglomeration / magnetic separation tests were the same as with magnetic coating. Best conditions for co-agglomeration on single minerals were pH=8, dodecylamine 2 kg/t, kerosene 4 L/t. Tests on mineral mixture reveals that the MgCO3-grade increases with dodecylamine but the yield drops.

Cite this record

Nikolaos Koukoulis, Athens, Greece, Georgios Anastassakis (2022). Reprocessing of magnesite beneficiation waste to recover mineral value and minimise environmental footprint. SUSTAINABLE EXTRACTION AND PROCESSING OF RAW MATERIALS, 3(3), 49–55. https://doi.org/10.58903/c16182118

Copy in another style

Koukoulis, N., Greece, A., & Anastassakis, G. (2022). Reprocessing of magnesite beneficiation waste to recover mineral value and minimise environmental footprint. SUSTAINABLE EXTRACTION AND PROCESSING OF RAW MATERIALS, 3(3), 49–55. https://doi.org/10.58903/c16182118
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.