We use a few cookies

Essential cookies keep the library working. With your permission, we'd also like to use analytics to see what's useful and improve the experience. Read our Privacy Policy or Cookie Policy.

Skip to main content
Home/e-Resources/Civil & Construction Engineering/Workability, microstructure, strength properties and durability properties of graphene oxide reinforced cement paste
PeriodicalsCivil & Construction Engineering

Workability, microstructure, strength properties and durability properties of graphene oxide reinforced cement paste

Checking your access to this record.

Abstract & Overview

Graphene oxide (GO) is one of the prominent nanomaterial, this has been utilised in the cement composite materials. Graphene oxide represents unprecedented range of properties with a potential to enhance the strength and toughness of cement-based composites. In this study, the influence of graphene oxide was evaluated on the workability, microstructure, strength and durability properties of the fresh and hardened cement composites. Different percentages of graphene oxide were added at 0wt%, 0.01wt%, 0.02wt%, 0.03wt% and 0.04wt% by weight of cement. Workability in terms of fluidity, setting time and viscosity tests were conducted to the fresh GO-cement paste samples. Compressive and flexural strength tests were conducted to the hardened GO-cement paste samples at 28 days. Through scanning electron microscopy (SEM), morphology and microstructure of hardened cement paste were investigated and XRD technique was assisted in identifying the crystalline materials and studying the phase composition of cement composites. Results exhibited that, graphene oxide addition increases the viscosity, decreases the fluidity and shortens the setting time of the cement paste. Increased compressive and flexural strength results were appeared due to the addition of graphene oxide at different dosages. At 0.04wt% of graphene oxide dosage, the compressive strength was increased by 46.6% and flexural strength was increased by 75% than normal cement paste at 28 days. Water permeability of the cement composite specimens was highly reduced due to the graphene oxide reinforced infiltration barrier, which leads to the improvement in durability.

Cite this record

Chandra Sekhar Reddy Indukuri, Ruben Nerella, Sri Rama Chand Madduru (2020). Workability, microstructure, strength properties and durability properties of graphene oxide reinforced cement paste. Australian Journal of Civil Engineering, 18(1), 73–81. https://doi.org/10.1080/14488353.2020.1721952

Copy in another style

Indukuri, C. S. R., Nerella, R., & Madduru, S. R. C. (2020). Workability, microstructure, strength properties and durability properties of graphene oxide reinforced cement paste. Australian Journal of Civil Engineering, 18(1), 73–81. https://doi.org/10.1080/14488353.2020.1721952
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.