Abstract & Overview

Inconel 718 is a precipitation strengthened, nickel-based super alloy of interest for the Additive Manufacturing (AM) of low volume, complex parts to reduce production time and cost compared to conventional subtractive processes. The AM process involves repeated rapid melting, solidification and reheating, which exposes the material to non-equilibrium conditions that affect elemental segregation and the subsequent formation of solidification phases, either beneficial or detrimental. These variations are difficult to characterize due to the small length scale within the micron sized melt pool. To understand how the non-equilibrium conditions affect the initial solidification phases and their critical temperatures, a multi-length scale, multi modal approach has been taken to evaluate various methods for identifying the initial phases formed in the as-built Inconel 718 produced by laser-powder bed fusion (L-PBF) additive manufacturing (AM). Using a range of characterization tools from the bulk differential thermal analysis (DTA) and x-ray diffraction (XRD) to spatially resolved images using a variety of electron microscopy tools, a better understanding is obtained of how these minor phases can be properly identified regarding the amount and size, morphology and distribution. Using the most promising characterization techniques for investigation of the as-built specimens, those techniques were used to evaluate the specimens after various heat treatments. During the sequence of heat treatments, the initial as-built dendritic structures recrystallized into well-defined grains whose size was dependent on the temperature. Although the resulting strength was similar in all heat treated specimens, the elongation increased as the grain size was refined due to differences in the precipitated phase distribution and morphology.

Cite this record

Judy A. Schneider, Laura Farris, Gert Nolze, Stefan Reinsch, Grzegorz Cios, Tomasz Tokarski, et al. (2022). Microstructure Evolution in Inconel 718 Produced by Powder Bed Fusion Additive Manufacturing. Journal of Manufacturing and Materials Processing, 6(1), 20–20. https://doi.org/10.3390/jmmp6010020

Copy in another style

Schneider, J. A., Farris, L., Nolze, G., Reinsch, S., Cios, G., Tokarski, T., & Thompson, S. (2022). Microstructure Evolution in Inconel 718 Produced by Powder Bed Fusion Additive Manufacturing. Journal of Manufacturing and Materials Processing, 6(1), 20–20. https://doi.org/10.3390/jmmp6010020
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.