Abstract & Overview
The pyrolysis behavior of PVC was investigated by pyrolysis-gas chromatography-mass spectrometry(GC-MS) in the presence of helium.GC-MS was used for the qualitative and semi-quantitative analysis of the pyrolysis products of PVC at 300,400,500,600,700,800 and 900 ℃,respectively.Altogether 40 pyrolysis products were detected,including hydrogen chloride,benzene,naphthalene,biphenyl,and phenanthrene.The results indicated that volatile substances,such as hydrogen chloride and benzene,were released from parent compound under 600 ℃.Moreover,with an increasing pyrolysis temperature,complicated pyrolysis products appeared,and the content of harmful substances,such as naphthalene,biphenyl and phenanthrene,were also increased.According to the relative content and category of the pyrolysis products,the technology for pyrolysis of PVC in different temperature ranges should be applied to lower the pyrolysis temperature and increase the pyrolysis efficiency.