Home/e-Resources/Electrical Engineering/Impact of curing temperatures and alkaline activators on compressive strength and porosity of ternary blended geopolymer mortars
PeriodicalsElectrical Engineering

Impact of curing temperatures and alkaline activators on compressive strength and porosity of ternary blended geopolymer mortars

Checking your access to this record.

Abstract & Overview

Impact of changing temperatures of curing (27, 60 and 90 °C) and types of alkaline activator solution on the properties of geopolymer mortars (GPMs) prepared by combining agricultural and industrial wastes including granulated-blast-furnace-slag (GBFS), fly-ash (FA), and palm-oil-fuel-ash (POFA) was examined. Sodium Hydroxide (NH), Sodium Silicate (NS) and NHNS alkaline solutions were used as alkali activators. Proposed GPMs were synthesized using NH solution of molarity 8 M, ratios of alkaline solution to binder were 0.30, NS to NH was 3.0 and binder to fine aggregate (sand) was 1.5. The mechanical properties of the studied GPMs and the products of reaction were greatly sensitive to the variation of mix compositions, alkaline activators type, and temperatures of curing. Furthermore, the formation of crystalline calcium silicate hydrate (C-S-H), calcium aluminium silicate hydrate (C-A-S-H) together with additional amorphous gel led to the compressive strength enhancement of the GPMs as the content of FA was increased and activated with NS solution. A linear correlation was established between compressive strength, ultrasonic pulse velocity and porosity of the proposed GPMs.

Cite this record

Ziyad Kubba, Ghasan Fahim Huseien, Abdul Rahman Mohd Sam, Kwok Wei Shah, Mohammad Ali Asaad, Mohammad Ismail, et al. (2018). Impact of curing temperatures and alkaline activators on compressive strength and porosity of ternary blended geopolymer mortars. Case Studies in Construction Materials, 9, e00205–e00205. https://doi.org/10.1016/j.cscm.2018.e00205

Copy in another style

Kubba, Z., Huseien, G. F., Sam, A. R. M., Shah, K. W., Asaad, M. A., Ismail, M., Tahir, M. M., & Mirza, J. (2018). Impact of curing temperatures and alkaline activators on compressive strength and porosity of ternary blended geopolymer mortars. Case Studies in Construction Materials, 9, e00205–e00205. https://doi.org/10.1016/j.cscm.2018.e00205
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.