Abstract & Overview
Lowering the concentration of digestion sulfuric acid can greatly reduce emissions of spent acid and flue gas in the sulfate process for TiO_2 pigment production. The experiments conducted under a high liquid/solid ratio and a well stirred situation, showed that the reaction activity was considerable high even in 65%~80% sulfuric acid solutions. A liquid-phase digestion operation was realized by continuously adding dilute acid or water to ensure the fluidity of reaction slurry. Mechanic agitation was employed to enhance the mass transfer. Comparing the liquid-phase digestion with solid-phase digestion, the experimental results indicate that the diffusion of reactants through solid product layer significantly affects the digestion degree of ilmenite in a commercial solid-phase digestion operation. The SEM and EDS characteristics show that the product layer over the un-reacted core in liquid phase digestion is thinner and its structure is looser comparing with solid phase digestion. With an industrial acid/ore ratio of 1.4 and an acid concentration of 65%~75%, digestion degrees higher than 85% were obtained at 150℃ ~160℃ within 120 min. Titaniferous solution with a TiO_2 content of 116 kg/m~3 and a F value of 2.0 was obtained, which was suitable for the pigment production. The liquid-phase operation shortened the periodic time to 2~3 hours.