Aging temperature history has profound effect on the mechanical and corrosion behavior of 6061 Al/SiC composite. In order to understand the effect of aging on the corrosion resistance, the natural and artificial aging behavior of 15 vol. % 6061 Al-SiCP composites was studied using the aging treatment and the Brinell hardness measurements. The aging curves for the composite (T6 treated) were determined at various aging temperatures such as room temperature, 140, 160, 180, 200, 220, and 240°C. According to the peak hardness variation with temperature profile, it is found that the composite is underaged at 140°C and 160°C. Peak aging takes place at 180°C. Overaging takes place at 200°C, 220°C, and 240°C. The natural aging characteristics of the composite (T4 treated) are also studied using the Brinell hardness measurements.

Cite this record

Rajasekaran Saminathan, N.K. Udayashankar, Jagannath Nayak (2012). T4 and T6 Treatment of 6061 Al-15 Vol. % SiCP Composite. ISRN Materials Science, 2012, 1–5. https://doi.org/10.5402/2012/374719

Copy in another style

Saminathan, R., Udayashankar, N., & Nayak, J. (2012). T4 and T6 Treatment of 6061 Al-15 Vol. % SiCP Composite. ISRN Materials Science, 2012, 1–5. https://doi.org/10.5402/2012/374719