在高性能WC-Co的制备中,WC与Co均匀混合和C含量的严格控制具有重要意义。以偏钨酸铵、乙酸钴、重铬酸铵和炭黑为原料,通过喷雾干燥和直接还原碳化法制备WC-Co复合粉末,然后在钼丝炉中通入氢气对前驱体进行还原碳化制备WC-Co复合粉末。对制备好的WC-Co进行总碳含量测定,用X射线衍射进行相分析。研究了喷雾法制备WC复合粉末形貌粒度及碳化温度、碳化时间、配碳量对WC-Co粉末总碳量的影响。结果表明:WC复合粉末为球形粉末,平均颗粒度为50μm;当碳化温度在950℃、碳化时间为3.5h、配碳量为9%时,所得WC-Co复合粉末中WC与Co达到均匀的分布,且其实际总碳含量达到理论总碳量5.79%。

Cite this record

Author (2010). 喷雾干燥-直接碳化法制备WC-Co复合粉末. 粉末冶金技术, 28(4), 279–283. https://library.shubhaarti.com/content/ecd6391e-bcb0-49cb-9423-f8a98ba69967

Copy in another style

Author. (2010). 喷雾干燥-直接碳化法制备WC-Co复合粉末. 粉末冶金技术, 28(4), 279–283. https://library.shubhaarti.com/content/ecd6391e-bcb0-49cb-9423-f8a98ba69967
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.