Fracture resistance and surface roughness assessment of digitally fabricated interim bridges

Checking your access to this record.

Abstract & Overview

Purpose The aim of this study was to evaluate the fracture resistance and surface roughness of interim bridges with different span lengths fabricated using two additive manufacturing techniques: stereolithography (SLA) and digital light processing (DLP), and to compare them with conventionally milled restorations. Materials and Methods Specimens were allocated into 3 groups according to fabrication technique (SLA, DLP, and milling; n=24 per group) and further subdivided based on span length (3-unit, 4-unit, and 6-unit; n=8 per group). The interim bridges were cemented onto their corresponding models, mounted in a universal testing machine, and progressively loaded until fracture. For surface roughness evaluation, 30 specimens were produced and divided into 3 groups according to fabrication technique (n=10). Mean surface roughness (Ra) was measured using a non-contact optical profilometer before and after polishing. Results The SLA bridges demonstrated fracture resistance values of 367±52 N for 3-unit, 124±22 N for 4-unit, and 91±31 N for 6-unit restorations. The DLP group exhibited lower fracture resistance values, with 283±28 N for 3-unit, 85±8 N for 4-unit, and 106±33 N for 6-unit bridges. Prior to polishing, milled specimens showed the highest mean surface roughness (32±3 μm), followed by DLP (14±1 μm), whereas SLA specimens exhibited the lowest Ra values (4±2 μm). Conclusion Fracture resistance of milled bridges surpassed 3D printed bridges across different span lengths. Long span three-dimensional (3D) printed bridges did not meet the clinical requirements for initial fracture resistance of interim bridges. Digitally fabricated bridges have clinically acceptable surface roughness following standard polishing techniques .

Cite this record

Nour Abdelmohsen, Anna K. Weber, Ahmed Mahmoud Fouda, Christoph Bourauel (2026). Fracture resistance and surface roughness assessment of digitally fabricated interim bridges. Digital Dentistry Journal, 3(1), 100092–100092. https://doi.org/10.1016/j.ddj.2026.100092

Copy in another style

Abdelmohsen, N., Weber, A. K., Fouda, A. M., & Bourauel, C. (2026). Fracture resistance and surface roughness assessment of digitally fabricated interim bridges. Digital Dentistry Journal, 3(1), 100092–100092. https://doi.org/10.1016/j.ddj.2026.100092
Author names are used as deposited, so check their order before you submit.

Metadata is harvested from open-access indexes and can be incomplete. Check a citation against the published version before relying on it — see our open access & attribution policy.