由于ZrB2的独特晶体结构,使其兼有金属和陶瓷的许多优异的物理和化学性能,因此在许多领域得到广泛应用。本文利用共沉淀法制备A1(OH)3-Y(OH)3/ZrB2复合粉体,并研究其形成热力学条件。经过热力学计算并用实验验证得出:ZrB2悬浮液的pH值必须大于8.3,才符合Al3+与Y3+共沉淀所需热力学条件;当ZrB2悬浮液的pH值为9时,A1(OH)3-Y(OH)3/ZrB2复合粉体的壳-核结构最好。在溶液浓度较低的情况下,可以获得具有理想壳-核结构的A1(OH)3-Y(OH)3/ZrB2复合粉体,即c(Al3+)=0.017mol/L,c(Y3+)=0.010mol/L,分别接近于Al(NO3)3和Y(NO3)3浓度的热力学条件计算拟定值,即:0.012 60mol/L和0.007 56mol/L。

Cite this record

Author, Zhigang Wang (2012). 共沉淀法制备A1(OH) 3 -Y(OH) 3 /ZrB2复合粉体的热力学形成条件研究. 粉末冶金技术, 30(4), 250–254. https://doi.org/10.3969/j.issn.1001-3784.2012.04.002

Copy in another style

Author, & Wang, Z. (2012). 共沉淀法制备A1(OH) 3 -Y(OH) 3 /ZrB2复合粉体的热力学形成条件研究. 粉末冶金技术, 30(4), 250–254. https://doi.org/10.3969/j.issn.1001-3784.2012.04.002