Abstract & Overview
Subsea pipeline installation using the S-lay technique subjects suspended pipelines to cyclic wave-induced loading, making girth weld imperfections, particularly crater defects, possible locations for fatigue initiation. Existing industry standards, including API 1104 and DNV-ST-F101, permit weld crater depths of up to 4mm; however, these limits are largely based on offshore pipeline experience from developed regions. This study examined the applicability of the 4 mm crater depth criterion for shallow-water fields, where daylight operations of up to 12 hours require pipelines to remain suspended on lay barges. An analytical–numerical hybrid approach was adopted to evaluate API 5L X70 pipelines with diameters ranging from 16 inches to 24 inches under hydrodynamic loading conditions. Stress concentration factors were determined using the Peterson formulation, with a maximum value of 5.273 applied in the analysis. Environmental conditions were represented using a characteristic Forcados sea state with a wave height of 2.48 m, a wave period of 11.93 s, and water depths starting from 22m. The results showed that stresses increased while fatigue life decreased with increasing water depth. Despite this trend, Miner’s cumulative damage values remained extremely low, ranging from 10⁻³¹ to 10⁻⁶, well below the accepted failure threshold (D ≪ 0.1<1). The findings confirmed that the 4mm crater depth criterion is conservative for shallow-water S-lay operations, but caution is needed for deepwater applications due to increased stresses and damage with depth.