Abstract & Overview
In this research the AA1060 and AA3003 alloys were compared by their crystallographic texture, hardness and earing. Both alloy sheets were rolled, and heat treated by the same manufacturing route. The cold rolled samples had the strain of 1.94, then the subsequent heat treatment was carried out between 190 °C and 380 °C. The annealing temperatures were chosen in respect to the industrial annealing temperatures. After the experiments XRD evaluation was carried out to determine the crystallographic texture of the sheets. The XRD results were compared with the industry-known earing test’s and hardness test’s results. The results can be applied in the industry for the optimization of a given technology.