Abstract & Overview
PdGa, cubic, P2 13( no.198), a =4.89695(6)Å, V =117.4Å 3 , Z =4,R gt(F) =0.024, wRref(F 2 ) =0.035, T =295 K. Source of materialLarge single crystals of PdGa were obtained by Czochralski growth from the melt as described in [1].The melt consisted of Pd (99.9 %, ChemPur) and Ga (99.99 %, ChemPur) in an atomic ratio of 45:55.The metals were pre-reacted in glassy carbon crucibles under inert argon atmosphere in ahigh-frequency induction furnace.Single crystals used in this study were obtained from the bottom of the as grown Czochralski crystal and were annealed at 800 °Cfor 24 hindynamic vacuum at 10 -6 mbar prior to the X-ray diffraction experiments.For the lattice parameter determination a small part of the bottom of the large crystal was crushed and an-