Abstract & Overview
Biomass molding fuel was prepared with both tar as binder and corn straw as raw materials. The effects of tar content, moisture content, molding pressure, material granularity and molding temperature on mechanical properties of molding fuel were studied. The results show that when the tar content increases from 0% to 12%, the falling strength of the molding fuel increases from 83.18% to 99.99%, and the density increases from 1.06 g/cm 3 to 1.36 g/cm 3 ; when the water content increases from 4% to 20%, the falling strength increases from 90.56% to 97.15%, and the density decreases gradually; when the molding pressure increases from 2 MPa to 4 MPa, the falling strength decreases by 0.33% and the density has no obvious change; when the material granularity increases from small particle size to 3 mm, the falling strength and density decrease; Increasing the molding temperature is beneficial to increase the falling strength and density.