Abstract & Overview
Two solvent impregnated activated carbon materials were prepared for uranium recovery from itsaqueous sulfate solutions using tridodecylamine (TDA) and tributyl phosphate (TBP). This was achievedby direct adsorption of each extractant onto the solid phase (dry method). The obtained adsorbentsdemonstrated that the loading capacity of TDA and TBP have attained 0.69g and 0.85g per 1g activatedcarbon (AC) respectively which were characterized by means of Scanning Electron Microscopy (SEM)and Fourier Transform Infrared Spectroscopy (FTIR). For the two materials, the relevant factors such ascontact time, solution pH, initial uranium ion concentration, volume of aqueous solution to the weight ofthe impregnated activated carbon ratio and the extraction temperature were optimized by equilibrium batchexperiments using uranium synthetic sulfate solution. The obtained uranium loaded from the latter on 1gof each of TDA-AC and TBP-AC was 45mg and 89mg respectively. Desorption of the loaded uraniumwas carried out using hydrochloric acid which was found to be 66% for TDA-AC and 93.5% for TBPACrespectively. Based on the obtained optimum factors, the practical applicability of the two developedimpregnated solid phases was then examined upon a uranium sulfate leach liquor prepared from AbuZeneima uraniferous mineralization.